The Stability of LSF-YSZ Electrodes Prepared by Infiltration
Penn collection
Degree type
Discipline
Subject
strontium compounds
yttrium compounds
zirconium compounds
electrodes
composite materials
calcination
lattice constants
electrical resistivity
anodisation
scanning electron microscopy
ageing
current density
sintering
melt infiltration
porous materials
ceramics
Funder
Grant number
License
Copyright date
Distributor
Related resources
Author
Contributor
Abstract
Composite electrodes were prepared by adding 40 wt % La0.8Sr0.2FeO3 (LSF) into porous yttria-stabilized zirconia (YSZ) and their performance was studied as a function of time and calcination temperature. X-ray diffraction (XRD) patterns of the LSF-YSZ composites indicated an expanded lattice parameter after calcination above 1523 K, suggesting that Zr reacted with the LSF to form a Zr-doped perovskite; but XRD provided no evidence for reaction between LSF and YSZ after calcination at 1373 K or after operation for 1000 h at 973 K and 700 h at 1073 K. A composite of 40 wt % La0.8Sr0.2Fe0.9Zr0.1O3 in YSZ showed reasonable performance at 973 K, with an area-specific resistance (ASR) of 0.22 Ω cm2. Based on symmetric-cell measurements, electrodes calcined at 1123 K showed an initial ASR of 0.13 Ω cm2 at 973 K but this increased linearly with time to 0.55 Ω cm2 after 2500 h at 973 K. However, the ASR depended strongly on current density, decreasing dramatically under both anodic and cathodic polarization. Electrodes calcined at 1373 K showed an ASR of 2.5 Ω cm2 at 973 K but this value also decreased dramatically under polarization. Scanning electron microcopy images demonstrate that aging at 973 K and calcination at 1373 K cause significant sintering of the LSF. It is therefore suggested that deactivation is caused by morphological changes, rather than solid-state reactions, with a dense layer of LSF forming over the YSZ substrate.